Physical Vapor Deposit (PVD)


Physical Vapor Deposit (PVD)

 

Coating Layer

Physical properties

Application

Micro-hardness

HV(50g)

Coating Color

Max. Working Temperature

Thickness

Key Characteristics

TIN

2000

Gold

600°C

4μ

Good general purpose, good lubrication.

Turning, milling Carbon Steel and Stainless steel.

TICN

3000

Gray

400°C

4μ

High hardness, good wear resistance, enhanced toughness.

Turning Carbon Steel and Alloyed Steel.

TIALN

(FUTURA NANO)

3300

Dark purple

900°C

3μ

Good general purpose, oxidation resistance.

Turning, milling Carbon Steel, Stainless Steel and Cast Iron.

TIALN-Muti Layer

3500

Dark

1100°C

4-6μ

High hardness, good wear resistance, heat oxidation resistance.

Turning, milling, drilling Carbon Steel, Alloyed Steel, Stainless Steel, Harden Steel and Cast Iron.

AT4Y

(multilayer coating)

3800

Dark purple and yellow

800°C

4-5μ

Containing aluminous element, heat oxidation resistance.

Suit for lubrication and dry type of turning, milling and drilling hard alloy and cast iron.

TRY

(multilayer coating)

3800

Violet hue

1100°C

4-7μ

Superhard nano-composite coatings, Low friction coefficientheat oxidation resistance.

Turning, milling and drilling stainless, tool steel, chrome vanadium steel and free cutting steel.

S

3400

Brown coal

900°C

2-4μ

Heat oxidation resistance, high hardness, good wear resistance.

Long lasting, suit for high temperature, machining heat treatment material above HRC60.

E

3200

Brown coal

800°C

2-5μ

High hardness, oxidation resistance, Low friction coefficient.

Suit for abrasive or stickiness materials, machining heat treatment alloyed steel HRC 50~62.

 

Inserts coated TIALN all used process FUTURA-NANO other process of TIALN coating need customer required.

Above multilayer coating is outer-layer as express.